Mitigating stress corrosion cracking and irradiation defects in OdS austenitic alloys by laser shock peening

Xueliang Yan, Yongfeng Lu, Michael Nastasi, Bai Cui

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Original languageEnglish (US)
Title of host publicationAISTech 2018 Proceedings - Iron and Steel Technology Conference and Exposition
PublisherAssociation for Iron and Steel Technology, AISTECH
Number of pages1
ISBN (Electronic)9781935117728
Publication statusPublished - Jan 1 2018
EventAISTech 2018 Iron and Steel Technology Conference and Exposition - Philadelphia, United States
Duration: May 7 2018May 10 2018

Publication series

NameAISTech - Iron and Steel Technology Conference Proceedings
Volume2018-May
ISSN (Print)1551-6997

Conference

ConferenceAISTech 2018 Iron and Steel Technology Conference and Exposition
CountryUnited States
CityPhiladelphia
Period5/7/185/10/18

ASJC Scopus subject areas

  • Industrial and Manufacturing Engineering

Cite this

Yan, X., Lu, Y., Nastasi, M., & Cui, B. (2018). Mitigating stress corrosion cracking and irradiation defects in OdS austenitic alloys by laser shock peening. In AISTech 2018 Proceedings - Iron and Steel Technology Conference and Exposition (AISTech - Iron and Steel Technology Conference Proceedings; Vol. 2018-May). Association for Iron and Steel Technology, AISTECH.