Mitigating stress corrosion cracking and irradiation defects in ods austenitic alloys by laser shock peening

Xueliang Yan, Yongfeng Lu, Michael Nastasi, Bai Cui

Research output: Contribution to journalConference article

Original languageEnglish (US)
Number of pages1
JournalTransactions of the American Nuclear Society
Volume118
StatePublished - Jan 1 2018
Event2018 Transactions of the American Nuclear Society, ANS 2018 and Embedded Topical Meeting Nuclear Fuels and Structural Materials - Philadelphia, United States
Duration: Jun 17 2018Jun 21 2018

Fingerprint

Shot peening
Stress corrosion cracking
Irradiation
Defects
Lasers

ASJC Scopus subject areas

  • Nuclear Energy and Engineering
  • Safety, Risk, Reliability and Quality

Cite this

Mitigating stress corrosion cracking and irradiation defects in ods austenitic alloys by laser shock peening. / Yan, Xueliang; Lu, Yongfeng; Nastasi, Michael; Cui, Bai.

In: Transactions of the American Nuclear Society, Vol. 118, 01.01.2018.

Research output: Contribution to journalConference article

@article{fe0bfcba773f47629361c79b01f243b3,
title = "Mitigating stress corrosion cracking and irradiation defects in ods austenitic alloys by laser shock peening",
author = "Xueliang Yan and Yongfeng Lu and Michael Nastasi and Bai Cui",
year = "2018",
month = "1",
day = "1",
language = "English (US)",
volume = "118",
journal = "Transactions of the American Nuclear Society",
issn = "0003-018X",

}

TY - JOUR

T1 - Mitigating stress corrosion cracking and irradiation defects in ods austenitic alloys by laser shock peening

AU - Yan, Xueliang

AU - Lu, Yongfeng

AU - Nastasi, Michael

AU - Cui, Bai

PY - 2018/1/1

Y1 - 2018/1/1

UR - http://www.scopus.com/inward/record.url?scp=85062991005&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85062991005&partnerID=8YFLogxK

M3 - Conference article

AN - SCOPUS:85062991005

VL - 118

JO - Transactions of the American Nuclear Society

JF - Transactions of the American Nuclear Society

SN - 0003-018X

ER -