Mechanical properties of heat-treated composite resin restorative materials

D. A. Covey, S. R. Tahaney, J. M. Davenport

Research output: Contribution to journalArticle

23 Citations (Scopus)

Abstract

Clinical methods for heat treating composite resin restorations have been developed. In this investigation, the effect of heat treatments on the diametral tensile strength of composite resin was determined. The composite resin restorative materials were selected according to the manufacturers' suggested use for anterior or posterior teeth, filler particle composition, and light-cured or chemical polymerization. Samples were prepared according to American Dental Association specification No. 27, and heat treatments were accomplished with a Coltene DI 500 oven for curing at approximately 120 ° C for 7 minutes. Heat treatment substantially increased the diametral tensile strength tested, with the exception of the anterior hybrid particle (p < 0.05). Composite resins with fine-particle inorganic fillers were significantly stronger than hybrid and microfilled composite resins.

Original languageEnglish (US)
Pages (from-to)458-461
Number of pages4
JournalThe Journal of prosthetic dentistry
Volume68
Issue number3
DOIs
StatePublished - Sep 1992

Fingerprint

Composite Resins
Hot Temperature
Tensile Strength
American Dental Association
Polymerization
Tooth
Light

ASJC Scopus subject areas

  • Oral Surgery

Cite this

Mechanical properties of heat-treated composite resin restorative materials. / Covey, D. A.; Tahaney, S. R.; Davenport, J. M.

In: The Journal of prosthetic dentistry, Vol. 68, No. 3, 09.1992, p. 458-461.

Research output: Contribution to journalArticle

Covey, D. A. ; Tahaney, S. R. ; Davenport, J. M. / Mechanical properties of heat-treated composite resin restorative materials. In: The Journal of prosthetic dentistry. 1992 ; Vol. 68, No. 3. pp. 458-461.
@article{a39a31c4cb204b98aef54e39cba41fdd,
title = "Mechanical properties of heat-treated composite resin restorative materials",
abstract = "Clinical methods for heat treating composite resin restorations have been developed. In this investigation, the effect of heat treatments on the diametral tensile strength of composite resin was determined. The composite resin restorative materials were selected according to the manufacturers' suggested use for anterior or posterior teeth, filler particle composition, and light-cured or chemical polymerization. Samples were prepared according to American Dental Association specification No. 27, and heat treatments were accomplished with a Coltene DI 500 oven for curing at approximately 120 ° C for 7 minutes. Heat treatment substantially increased the diametral tensile strength tested, with the exception of the anterior hybrid particle (p < 0.05). Composite resins with fine-particle inorganic fillers were significantly stronger than hybrid and microfilled composite resins.",
author = "Covey, {D. A.} and Tahaney, {S. R.} and Davenport, {J. M.}",
year = "1992",
month = "9",
doi = "10.1016/0022-3913(92)90410-C",
language = "English (US)",
volume = "68",
pages = "458--461",
journal = "Journal of Prosthetic Dentistry",
issn = "0022-3913",
publisher = "Mosby Inc.",
number = "3",

}

TY - JOUR

T1 - Mechanical properties of heat-treated composite resin restorative materials

AU - Covey, D. A.

AU - Tahaney, S. R.

AU - Davenport, J. M.

PY - 1992/9

Y1 - 1992/9

N2 - Clinical methods for heat treating composite resin restorations have been developed. In this investigation, the effect of heat treatments on the diametral tensile strength of composite resin was determined. The composite resin restorative materials were selected according to the manufacturers' suggested use for anterior or posterior teeth, filler particle composition, and light-cured or chemical polymerization. Samples were prepared according to American Dental Association specification No. 27, and heat treatments were accomplished with a Coltene DI 500 oven for curing at approximately 120 ° C for 7 minutes. Heat treatment substantially increased the diametral tensile strength tested, with the exception of the anterior hybrid particle (p < 0.05). Composite resins with fine-particle inorganic fillers were significantly stronger than hybrid and microfilled composite resins.

AB - Clinical methods for heat treating composite resin restorations have been developed. In this investigation, the effect of heat treatments on the diametral tensile strength of composite resin was determined. The composite resin restorative materials were selected according to the manufacturers' suggested use for anterior or posterior teeth, filler particle composition, and light-cured or chemical polymerization. Samples were prepared according to American Dental Association specification No. 27, and heat treatments were accomplished with a Coltene DI 500 oven for curing at approximately 120 ° C for 7 minutes. Heat treatment substantially increased the diametral tensile strength tested, with the exception of the anterior hybrid particle (p < 0.05). Composite resins with fine-particle inorganic fillers were significantly stronger than hybrid and microfilled composite resins.

UR - http://www.scopus.com/inward/record.url?scp=0026927947&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0026927947&partnerID=8YFLogxK

U2 - 10.1016/0022-3913(92)90410-C

DO - 10.1016/0022-3913(92)90410-C

M3 - Article

C2 - 1432761

AN - SCOPUS:0026927947

VL - 68

SP - 458

EP - 461

JO - Journal of Prosthetic Dentistry

JF - Journal of Prosthetic Dentistry

SN - 0022-3913

IS - 3

ER -