This study evaluates hydrated lime-treated hot-mix asphalt (HMA) mixtures through various laboratory tests, including the dynamic modulus test and performance tests to characterize permanent deformation and fatigue damage resistance both in displacement-controlled and force-controlled modes. Two different asphalt mixtures - the asphalt concrete mixture and the fine aggregate asphalt matrix mixture - which differ only in the amount of additional hydrated lime (0.5-3.0%), are tested. Test results demonstrate material-specific damage characteristics of hydrated lime and the existence of a more appropriate amount of hydrated lime to be added to the HMA mixtures than the current typical application rate such as the addition of 1.0% lime to dry or pre-moistened aggregates. In addition, the newly released Mechanistic-Empirical Pavement Design Guide (MEPDG) is used for predicting pavement performance related to hydrated lime content. The MEPDG analysis results show that damage prediction models implemented in the current MEPDG are limited to accurately predicting material-specific damage characteristics. Mechanistic models that consider material-specific crack phenomenon and fracture behavior should be pursued.

Original languageEnglish (US)
Pages (from-to)538-544
Number of pages7
JournalConstruction and Building Materials
Volume24
Issue number4
DOIs
StatePublished - Apr 1 2010

Fingerprint

Hydrated lime
Asphalt mixtures
Pavements
asphalt
Asphalt concrete
Concrete mixtures
Fatigue damage
Asphalt
Lime
Cracks

Keywords

  • Hot-mix asphalt
  • Hydrated lime
  • Mechanistic-Empirical Pavement Design Guide
  • Pavement performance

ASJC Scopus subject areas

  • Civil and Structural Engineering
  • Building and Construction
  • Materials Science(all)

Cite this

Material-specific effects of hydrated lime on the properties and performance behavior of asphalt mixtures and asphaltic pavements. / Aragão, Francisco Thiago Sacramento; Lee, Junghun; Kim, Yong-Rak; Karki, Pravat.

In: Construction and Building Materials, Vol. 24, No. 4, 01.04.2010, p. 538-544.

Research output: Contribution to journalArticle

@article{f02ddec55c4a41c1ac51b6e276701830,
title = "Material-specific effects of hydrated lime on the properties and performance behavior of asphalt mixtures and asphaltic pavements",
abstract = "This study evaluates hydrated lime-treated hot-mix asphalt (HMA) mixtures through various laboratory tests, including the dynamic modulus test and performance tests to characterize permanent deformation and fatigue damage resistance both in displacement-controlled and force-controlled modes. Two different asphalt mixtures - the asphalt concrete mixture and the fine aggregate asphalt matrix mixture - which differ only in the amount of additional hydrated lime (0.5-3.0{\%}), are tested. Test results demonstrate material-specific damage characteristics of hydrated lime and the existence of a more appropriate amount of hydrated lime to be added to the HMA mixtures than the current typical application rate such as the addition of 1.0{\%} lime to dry or pre-moistened aggregates. In addition, the newly released Mechanistic-Empirical Pavement Design Guide (MEPDG) is used for predicting pavement performance related to hydrated lime content. The MEPDG analysis results show that damage prediction models implemented in the current MEPDG are limited to accurately predicting material-specific damage characteristics. Mechanistic models that consider material-specific crack phenomenon and fracture behavior should be pursued.",
keywords = "Hot-mix asphalt, Hydrated lime, Mechanistic-Empirical Pavement Design Guide, Pavement performance",
author = "Arag{\~a}o, {Francisco Thiago Sacramento} and Junghun Lee and Yong-Rak Kim and Pravat Karki",
year = "2010",
month = "4",
day = "1",
doi = "10.1016/j.conbuildmat.2009.10.005",
language = "English (US)",
volume = "24",
pages = "538--544",
journal = "Construction and Building Materials",
issn = "0950-0618",
publisher = "Elsevier Limited",
number = "4",

}

TY - JOUR

T1 - Material-specific effects of hydrated lime on the properties and performance behavior of asphalt mixtures and asphaltic pavements

AU - Aragão, Francisco Thiago Sacramento

AU - Lee, Junghun

AU - Kim, Yong-Rak

AU - Karki, Pravat

PY - 2010/4/1

Y1 - 2010/4/1

N2 - This study evaluates hydrated lime-treated hot-mix asphalt (HMA) mixtures through various laboratory tests, including the dynamic modulus test and performance tests to characterize permanent deformation and fatigue damage resistance both in displacement-controlled and force-controlled modes. Two different asphalt mixtures - the asphalt concrete mixture and the fine aggregate asphalt matrix mixture - which differ only in the amount of additional hydrated lime (0.5-3.0%), are tested. Test results demonstrate material-specific damage characteristics of hydrated lime and the existence of a more appropriate amount of hydrated lime to be added to the HMA mixtures than the current typical application rate such as the addition of 1.0% lime to dry or pre-moistened aggregates. In addition, the newly released Mechanistic-Empirical Pavement Design Guide (MEPDG) is used for predicting pavement performance related to hydrated lime content. The MEPDG analysis results show that damage prediction models implemented in the current MEPDG are limited to accurately predicting material-specific damage characteristics. Mechanistic models that consider material-specific crack phenomenon and fracture behavior should be pursued.

AB - This study evaluates hydrated lime-treated hot-mix asphalt (HMA) mixtures through various laboratory tests, including the dynamic modulus test and performance tests to characterize permanent deformation and fatigue damage resistance both in displacement-controlled and force-controlled modes. Two different asphalt mixtures - the asphalt concrete mixture and the fine aggregate asphalt matrix mixture - which differ only in the amount of additional hydrated lime (0.5-3.0%), are tested. Test results demonstrate material-specific damage characteristics of hydrated lime and the existence of a more appropriate amount of hydrated lime to be added to the HMA mixtures than the current typical application rate such as the addition of 1.0% lime to dry or pre-moistened aggregates. In addition, the newly released Mechanistic-Empirical Pavement Design Guide (MEPDG) is used for predicting pavement performance related to hydrated lime content. The MEPDG analysis results show that damage prediction models implemented in the current MEPDG are limited to accurately predicting material-specific damage characteristics. Mechanistic models that consider material-specific crack phenomenon and fracture behavior should be pursued.

KW - Hot-mix asphalt

KW - Hydrated lime

KW - Mechanistic-Empirical Pavement Design Guide

KW - Pavement performance

UR - http://www.scopus.com/inward/record.url?scp=74649083270&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=74649083270&partnerID=8YFLogxK

U2 - 10.1016/j.conbuildmat.2009.10.005

DO - 10.1016/j.conbuildmat.2009.10.005

M3 - Article

VL - 24

SP - 538

EP - 544

JO - Construction and Building Materials

JF - Construction and Building Materials

SN - 0950-0618

IS - 4

ER -