Abstract

The purpose of this study was to evaluate the effectiveness of various surface treatments used to enhance the bond strength of resin cements to two different laboratory-processed composite resins. Seventy specimens of a microfilled composite resin (Concept) and 70 specimens of a micro-hybrid composite resin (Herculite XRV) were fabricated in metal wells and subjected to heat (250°F) and pressure (85 psi) curing. An additional 70 specimens of each material were fabricated in the shape of disks and also subjected to the same heat/pressure curing. All composite resins were subjected to one of seven treatment regimens. The like-treated specimens were then bonded together using dual-curing resin cement and a uniform seating force (106 gm). After 7 days, bonded specimens were thermocycled 1000 times at 5 and 55°C, and debond shear strengths were determined on a Universal Testing Machine. The use of microabrasion (50 μm aluminum oxide at 60 psi) and ceramic layer deposition (30 μm aluminum oxide with a ceramic additive at 75 psi) consistently improved the shear bond strength of the resin cements to both composite resins. The other treatment combinations provided varying effects. In conclusion, microabrasion or ceramic layer deposition are preferred methods to enhance the bond of resin cements to composite resins.

Original languageEnglish (US)
Pages (from-to)249-256
Number of pages8
JournalOperative dentistry
Volume21
Issue number6
StatePublished - Nov 1 1996

Fingerprint

Composite Resins
Hot Temperature
Resin Cements
Ceramics
Shear Strength
Aluminum Oxide
Self-Curing of Dental Resins
Pressure
Metals

ASJC Scopus subject areas

  • Medicine(all)
  • Dentistry(all)

Cite this

Imamura, G. M., Reinhardt, J. W., Boyer, D. B., & Swift, E. J. (1996). Enhancement of resin bonding to heat-cured composite resin. Operative dentistry, 21(6), 249-256.

Enhancement of resin bonding to heat-cured composite resin. / Imamura, G. M.; Reinhardt, J. W.; Boyer, D. B.; Swift, E. J.

In: Operative dentistry, Vol. 21, No. 6, 01.11.1996, p. 249-256.

Research output: Contribution to journalArticle

Imamura, GM, Reinhardt, JW, Boyer, DB & Swift, EJ 1996, 'Enhancement of resin bonding to heat-cured composite resin', Operative dentistry, vol. 21, no. 6, pp. 249-256.
Imamura GM, Reinhardt JW, Boyer DB, Swift EJ. Enhancement of resin bonding to heat-cured composite resin. Operative dentistry. 1996 Nov 1;21(6):249-256.
Imamura, G. M. ; Reinhardt, J. W. ; Boyer, D. B. ; Swift, E. J. / Enhancement of resin bonding to heat-cured composite resin. In: Operative dentistry. 1996 ; Vol. 21, No. 6. pp. 249-256.
@article{2332c12c790641cd951750b3f82a850b,
title = "Enhancement of resin bonding to heat-cured composite resin",
abstract = "The purpose of this study was to evaluate the effectiveness of various surface treatments used to enhance the bond strength of resin cements to two different laboratory-processed composite resins. Seventy specimens of a microfilled composite resin (Concept) and 70 specimens of a micro-hybrid composite resin (Herculite XRV) were fabricated in metal wells and subjected to heat (250°F) and pressure (85 psi) curing. An additional 70 specimens of each material were fabricated in the shape of disks and also subjected to the same heat/pressure curing. All composite resins were subjected to one of seven treatment regimens. The like-treated specimens were then bonded together using dual-curing resin cement and a uniform seating force (106 gm). After 7 days, bonded specimens were thermocycled 1000 times at 5 and 55°C, and debond shear strengths were determined on a Universal Testing Machine. The use of microabrasion (50 μm aluminum oxide at 60 psi) and ceramic layer deposition (30 μm aluminum oxide with a ceramic additive at 75 psi) consistently improved the shear bond strength of the resin cements to both composite resins. The other treatment combinations provided varying effects. In conclusion, microabrasion or ceramic layer deposition are preferred methods to enhance the bond of resin cements to composite resins.",
author = "Imamura, {G. M.} and Reinhardt, {J. W.} and Boyer, {D. B.} and Swift, {E. J.}",
year = "1996",
month = "11",
day = "1",
language = "English (US)",
volume = "21",
pages = "249--256",
journal = "Operative Dentistry",
issn = "0361-7734",
publisher = "Indiana University School of Dentistry",
number = "6",

}

TY - JOUR

T1 - Enhancement of resin bonding to heat-cured composite resin

AU - Imamura, G. M.

AU - Reinhardt, J. W.

AU - Boyer, D. B.

AU - Swift, E. J.

PY - 1996/11/1

Y1 - 1996/11/1

N2 - The purpose of this study was to evaluate the effectiveness of various surface treatments used to enhance the bond strength of resin cements to two different laboratory-processed composite resins. Seventy specimens of a microfilled composite resin (Concept) and 70 specimens of a micro-hybrid composite resin (Herculite XRV) were fabricated in metal wells and subjected to heat (250°F) and pressure (85 psi) curing. An additional 70 specimens of each material were fabricated in the shape of disks and also subjected to the same heat/pressure curing. All composite resins were subjected to one of seven treatment regimens. The like-treated specimens were then bonded together using dual-curing resin cement and a uniform seating force (106 gm). After 7 days, bonded specimens were thermocycled 1000 times at 5 and 55°C, and debond shear strengths were determined on a Universal Testing Machine. The use of microabrasion (50 μm aluminum oxide at 60 psi) and ceramic layer deposition (30 μm aluminum oxide with a ceramic additive at 75 psi) consistently improved the shear bond strength of the resin cements to both composite resins. The other treatment combinations provided varying effects. In conclusion, microabrasion or ceramic layer deposition are preferred methods to enhance the bond of resin cements to composite resins.

AB - The purpose of this study was to evaluate the effectiveness of various surface treatments used to enhance the bond strength of resin cements to two different laboratory-processed composite resins. Seventy specimens of a microfilled composite resin (Concept) and 70 specimens of a micro-hybrid composite resin (Herculite XRV) were fabricated in metal wells and subjected to heat (250°F) and pressure (85 psi) curing. An additional 70 specimens of each material were fabricated in the shape of disks and also subjected to the same heat/pressure curing. All composite resins were subjected to one of seven treatment regimens. The like-treated specimens were then bonded together using dual-curing resin cement and a uniform seating force (106 gm). After 7 days, bonded specimens were thermocycled 1000 times at 5 and 55°C, and debond shear strengths were determined on a Universal Testing Machine. The use of microabrasion (50 μm aluminum oxide at 60 psi) and ceramic layer deposition (30 μm aluminum oxide with a ceramic additive at 75 psi) consistently improved the shear bond strength of the resin cements to both composite resins. The other treatment combinations provided varying effects. In conclusion, microabrasion or ceramic layer deposition are preferred methods to enhance the bond of resin cements to composite resins.

UR - http://www.scopus.com/inward/record.url?scp=0030275966&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0030275966&partnerID=8YFLogxK

M3 - Article

C2 - 9227119

AN - SCOPUS:0030275966

VL - 21

SP - 249

EP - 256

JO - Operative Dentistry

JF - Operative Dentistry

SN - 0361-7734

IS - 6

ER -