Abstract

Previous studies have examined the relationship between total filler content in hybrid restorative composites and some of their mechanical properties. This investigation evaluated the effect of varying the amount of microfiller in an experimental hybrid composite on fracture toughness (single edge-notch technique) and diametral tensile strength. The microfiller content in the experimental hybrid composite was varied from 0-44 wt% for seven specimen groups, while the total filler content ranged from 77-84 wt%. It was found that 9 wt% microfiller loading produced the highest mean fracture toughness (1.33 MPa·m 1 2) and 44 wt% loading produced the lowest mean value (0.80 MPa·m 1 2). Only the 9 wt% microfiller content group differed significantly in fracture toughness from the other specimen groups. The diametral tensile strength displayed only small differences for the range of microfiller content studied, with mean values ranging from 42.1-49.6 MPa. Additional research on the viscoelastic properties of these heavily filled hybrid composites may provide some insight into the differences for the fracture toughness and diametral tensile strength results.

Original languageEnglish (US)
Pages (from-to)95-98
Number of pages4
JournalDental Materials
Volume9
Issue number2
DOIs
StatePublished - Mar 1993

Fingerprint

Tensile Strength
Fracture toughness
Tensile strength
Composite materials
Fillers
Mechanical properties
Research

ASJC Scopus subject areas

  • Materials Science(all)
  • Dentistry(all)
  • Mechanics of Materials

Cite this

Composite microfiller content and its effect on fracture toughness and diametral tensile strength. / Johnson, W. W.; Dhuru, V. B.; Brantley, W. A.

In: Dental Materials, Vol. 9, No. 2, 03.1993, p. 95-98.

Research output: Contribution to journalArticle

@article{336dee7af6ed433f9e197cd91b39ac58,
title = "Composite microfiller content and its effect on fracture toughness and diametral tensile strength",
abstract = "Previous studies have examined the relationship between total filler content in hybrid restorative composites and some of their mechanical properties. This investigation evaluated the effect of varying the amount of microfiller in an experimental hybrid composite on fracture toughness (single edge-notch technique) and diametral tensile strength. The microfiller content in the experimental hybrid composite was varied from 0-44 wt{\%} for seven specimen groups, while the total filler content ranged from 77-84 wt{\%}. It was found that 9 wt{\%} microfiller loading produced the highest mean fracture toughness (1.33 MPa·m 1 2) and 44 wt{\%} loading produced the lowest mean value (0.80 MPa·m 1 2). Only the 9 wt{\%} microfiller content group differed significantly in fracture toughness from the other specimen groups. The diametral tensile strength displayed only small differences for the range of microfiller content studied, with mean values ranging from 42.1-49.6 MPa. Additional research on the viscoelastic properties of these heavily filled hybrid composites may provide some insight into the differences for the fracture toughness and diametral tensile strength results.",
author = "Johnson, {W. W.} and Dhuru, {V. B.} and Brantley, {W. A.}",
year = "1993",
month = "3",
doi = "10.1016/0109-5641(93)90082-2",
language = "English (US)",
volume = "9",
pages = "95--98",
journal = "Dental Materials",
issn = "0109-5641",
publisher = "Elsevier Science",
number = "2",

}

TY - JOUR

T1 - Composite microfiller content and its effect on fracture toughness and diametral tensile strength

AU - Johnson, W. W.

AU - Dhuru, V. B.

AU - Brantley, W. A.

PY - 1993/3

Y1 - 1993/3

N2 - Previous studies have examined the relationship between total filler content in hybrid restorative composites and some of their mechanical properties. This investigation evaluated the effect of varying the amount of microfiller in an experimental hybrid composite on fracture toughness (single edge-notch technique) and diametral tensile strength. The microfiller content in the experimental hybrid composite was varied from 0-44 wt% for seven specimen groups, while the total filler content ranged from 77-84 wt%. It was found that 9 wt% microfiller loading produced the highest mean fracture toughness (1.33 MPa·m 1 2) and 44 wt% loading produced the lowest mean value (0.80 MPa·m 1 2). Only the 9 wt% microfiller content group differed significantly in fracture toughness from the other specimen groups. The diametral tensile strength displayed only small differences for the range of microfiller content studied, with mean values ranging from 42.1-49.6 MPa. Additional research on the viscoelastic properties of these heavily filled hybrid composites may provide some insight into the differences for the fracture toughness and diametral tensile strength results.

AB - Previous studies have examined the relationship between total filler content in hybrid restorative composites and some of their mechanical properties. This investigation evaluated the effect of varying the amount of microfiller in an experimental hybrid composite on fracture toughness (single edge-notch technique) and diametral tensile strength. The microfiller content in the experimental hybrid composite was varied from 0-44 wt% for seven specimen groups, while the total filler content ranged from 77-84 wt%. It was found that 9 wt% microfiller loading produced the highest mean fracture toughness (1.33 MPa·m 1 2) and 44 wt% loading produced the lowest mean value (0.80 MPa·m 1 2). Only the 9 wt% microfiller content group differed significantly in fracture toughness from the other specimen groups. The diametral tensile strength displayed only small differences for the range of microfiller content studied, with mean values ranging from 42.1-49.6 MPa. Additional research on the viscoelastic properties of these heavily filled hybrid composites may provide some insight into the differences for the fracture toughness and diametral tensile strength results.

UR - http://www.scopus.com/inward/record.url?scp=0027572486&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0027572486&partnerID=8YFLogxK

U2 - 10.1016/0109-5641(93)90082-2

DO - 10.1016/0109-5641(93)90082-2

M3 - Article

C2 - 8595849

AN - SCOPUS:0027572486

VL - 9

SP - 95

EP - 98

JO - Dental Materials

JF - Dental Materials

SN - 0109-5641

IS - 2

ER -