Ten popular disperse dyes with different energy levels and chemical constitutions were used to compare their exhaustion, color yield, and colorfastness on polylactide (PLA) and poly(ethylene terephthalate) (PET). Only two out of the 10 dyes had exhaustions higher than 80% on PLA at 2% owf. Five out of the 10 dyes had exhaustions less than 50%. All 10 dyes had more than 90% exhaustion on PET, whereas six of them had exhaustions of 98% or higher. There was no obvious pattern as for which energy level or which structure class provided dye exhaustion better than that of others. Although PLA had lower disperse dye exhaustion than that of PET, it had higher color yield. Based on the 10 dyes examined, the color yield of PLA was about 30% higher than that of PET. This means that even with low dye uptake, PLA could have a similar apparent shade depth as that of PET if the same dyeing conditions are applied. Our study supported that the lower reflectance, or reflectivity, of PLA contributes to the higher color yield of PLA than that of PET. A quantitative relation between the shade depth of PLA and PET based on their dye sorption was developed. Disperse dyes examined had lower washing and crocking fastness on PLA than on PET. The differences in class were about 0.5 to 1.0. If the comparison was based on the same dye uptake, the differences might be larger. The differences in light fastness between the two fibers were smaller than that in washing and crocking fastnesses. The light fastness of disperse dyes on PLA is expected to be even better if the comparison is based on the same dye uptake on both fibers.

Original languageEnglish (US)
Pages (from-to)3285-3290
Number of pages6
JournalJournal of Applied Polymer Science
Volume90
Issue number12
DOIs
StatePublished - Dec 13 2003

Fingerprint

Polyethylene Terephthalates
Polyethylene terephthalates
Coloring Agents
Dyes
Color
Washing
poly(lactide)
Electron energy levels
Fibers
Dyeing
Sorption

Keywords

  • Colorfastness
  • Dispersions
  • Dyes/pigments
  • Polyesters
  • Refractive index

ASJC Scopus subject areas

  • Chemistry(all)
  • Surfaces, Coatings and Films
  • Polymers and Plastics
  • Materials Chemistry

Cite this

Comparison of Disperse Dye Exhaustion, Color Yield, and Colorfastness between Polylactide and Poly(ethylene terephthalate). / Yang, Yiqi; Huda, Shah.

In: Journal of Applied Polymer Science, Vol. 90, No. 12, 13.12.2003, p. 3285-3290.

Research output: Contribution to journalArticle

@article{809ffb8ceb424f338c2bba6d2e8cbbb5,
title = "Comparison of Disperse Dye Exhaustion, Color Yield, and Colorfastness between Polylactide and Poly(ethylene terephthalate)",
abstract = "Ten popular disperse dyes with different energy levels and chemical constitutions were used to compare their exhaustion, color yield, and colorfastness on polylactide (PLA) and poly(ethylene terephthalate) (PET). Only two out of the 10 dyes had exhaustions higher than 80{\%} on PLA at 2{\%} owf. Five out of the 10 dyes had exhaustions less than 50{\%}. All 10 dyes had more than 90{\%} exhaustion on PET, whereas six of them had exhaustions of 98{\%} or higher. There was no obvious pattern as for which energy level or which structure class provided dye exhaustion better than that of others. Although PLA had lower disperse dye exhaustion than that of PET, it had higher color yield. Based on the 10 dyes examined, the color yield of PLA was about 30{\%} higher than that of PET. This means that even with low dye uptake, PLA could have a similar apparent shade depth as that of PET if the same dyeing conditions are applied. Our study supported that the lower reflectance, or reflectivity, of PLA contributes to the higher color yield of PLA than that of PET. A quantitative relation between the shade depth of PLA and PET based on their dye sorption was developed. Disperse dyes examined had lower washing and crocking fastness on PLA than on PET. The differences in class were about 0.5 to 1.0. If the comparison was based on the same dye uptake, the differences might be larger. The differences in light fastness between the two fibers were smaller than that in washing and crocking fastnesses. The light fastness of disperse dyes on PLA is expected to be even better if the comparison is based on the same dye uptake on both fibers.",
keywords = "Colorfastness, Dispersions, Dyes/pigments, Polyesters, Refractive index",
author = "Yiqi Yang and Shah Huda",
year = "2003",
month = "12",
day = "13",
doi = "10.1002/app.13062",
language = "English (US)",
volume = "90",
pages = "3285--3290",
journal = "Journal of Applied Polymer Science",
issn = "0021-8995",
publisher = "John Wiley and Sons Inc.",
number = "12",

}

TY - JOUR

T1 - Comparison of Disperse Dye Exhaustion, Color Yield, and Colorfastness between Polylactide and Poly(ethylene terephthalate)

AU - Yang, Yiqi

AU - Huda, Shah

PY - 2003/12/13

Y1 - 2003/12/13

N2 - Ten popular disperse dyes with different energy levels and chemical constitutions were used to compare their exhaustion, color yield, and colorfastness on polylactide (PLA) and poly(ethylene terephthalate) (PET). Only two out of the 10 dyes had exhaustions higher than 80% on PLA at 2% owf. Five out of the 10 dyes had exhaustions less than 50%. All 10 dyes had more than 90% exhaustion on PET, whereas six of them had exhaustions of 98% or higher. There was no obvious pattern as for which energy level or which structure class provided dye exhaustion better than that of others. Although PLA had lower disperse dye exhaustion than that of PET, it had higher color yield. Based on the 10 dyes examined, the color yield of PLA was about 30% higher than that of PET. This means that even with low dye uptake, PLA could have a similar apparent shade depth as that of PET if the same dyeing conditions are applied. Our study supported that the lower reflectance, or reflectivity, of PLA contributes to the higher color yield of PLA than that of PET. A quantitative relation between the shade depth of PLA and PET based on their dye sorption was developed. Disperse dyes examined had lower washing and crocking fastness on PLA than on PET. The differences in class were about 0.5 to 1.0. If the comparison was based on the same dye uptake, the differences might be larger. The differences in light fastness between the two fibers were smaller than that in washing and crocking fastnesses. The light fastness of disperse dyes on PLA is expected to be even better if the comparison is based on the same dye uptake on both fibers.

AB - Ten popular disperse dyes with different energy levels and chemical constitutions were used to compare their exhaustion, color yield, and colorfastness on polylactide (PLA) and poly(ethylene terephthalate) (PET). Only two out of the 10 dyes had exhaustions higher than 80% on PLA at 2% owf. Five out of the 10 dyes had exhaustions less than 50%. All 10 dyes had more than 90% exhaustion on PET, whereas six of them had exhaustions of 98% or higher. There was no obvious pattern as for which energy level or which structure class provided dye exhaustion better than that of others. Although PLA had lower disperse dye exhaustion than that of PET, it had higher color yield. Based on the 10 dyes examined, the color yield of PLA was about 30% higher than that of PET. This means that even with low dye uptake, PLA could have a similar apparent shade depth as that of PET if the same dyeing conditions are applied. Our study supported that the lower reflectance, or reflectivity, of PLA contributes to the higher color yield of PLA than that of PET. A quantitative relation between the shade depth of PLA and PET based on their dye sorption was developed. Disperse dyes examined had lower washing and crocking fastness on PLA than on PET. The differences in class were about 0.5 to 1.0. If the comparison was based on the same dye uptake, the differences might be larger. The differences in light fastness between the two fibers were smaller than that in washing and crocking fastnesses. The light fastness of disperse dyes on PLA is expected to be even better if the comparison is based on the same dye uptake on both fibers.

KW - Colorfastness

KW - Dispersions

KW - Dyes/pigments

KW - Polyesters

KW - Refractive index

UR - http://www.scopus.com/inward/record.url?scp=0242497213&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0242497213&partnerID=8YFLogxK

U2 - 10.1002/app.13062

DO - 10.1002/app.13062

M3 - Article

AN - SCOPUS:0242497213

VL - 90

SP - 3285

EP - 3290

JO - Journal of Applied Polymer Science

JF - Journal of Applied Polymer Science

SN - 0021-8995

IS - 12

ER -